Article 2054 is the lamination base of our water jet range, made in our own water jet interlining factory — a cloth built to be bonded to a shell rather than hung behind it. It is worth being clear about what this is not. It is not a garment lining. Nothing here is sewn in as a separate cloth for comfort or cover; the PA coating is activated under a fusing press and the interlining becomes part of the panel, so the body it gives is the panel's own body and the surface stays clean. That makes it useful wherever a soft shell would otherwise lose its line — jacket fronts, collar stands, cuffs, pocket flaps and the leading edges that take the most handling. It is a working cloth rather than a delicate one: it can be spread, layered and cut on a normal outerwear line without special handling. Typical buyers are outerwear factories building coats and casual jackets, uniform and workwear producers, and converters who bond the cloth to a face fabric before the garment is assembled. All of them are buying the same thing: a base that fuses predictably and holds its shape in the finished garment without making it feel heavy. - Two shades cover most shells — off white sits comfortably behind pale and natural face fabrics, black behind dark ones, so one article covers a mixed colour range without a second purchase order. - The standard roll width keeps offcuts down — it suits the way outerwear markers are usually laid, so fewer panels come off a narrow edge and less metreage is wasted per garment. - No special equipment on the line — the PA coating develops its bond on standard fusing presses, so your existing setup can be trialled as it stands rather than rebuilt around a new material.
Repeat processing is where an interlining earns or loses its reputation. The first roll of a new article is judged in the sample room; the third reorder is judged on the line, by cutters and fusing operators who notice a change in how the cloth handles long before anyone measures it. This article is built to survive that scrutiny. Rework falls when operators do not have to compensate for a material that changes character between batches. Through bonding and sewing the cloth holds a steady form. It does not creep under the press foot or pucker along the seam line, so the routine on the line stays the same from the first style of the season to the last, and the sewing room receives panels that align without trimming. None of this is visible in a single sample. It shows up in the four-hundredth metre and in the fourth reorder, which is why continuity of construction matters more than any one measurement. Because we run both the base cloth and the coating in one water jet interlining factory, the article you reorder is built the way the first shipment was built.
The bond is a process, not an ingredient. Face fabric is the first variable. A tightly woven, smoothly finished shell gives the adhesive less surface to key into than an open or brushed one, and a shell carrying a water-repellent finish can resist wetting unless the dwell is long enough. Bond on the shell you will actually run, in the finish you will actually receive, rather than on a stock swatch from the sample box. The second variable is cooling. Fusible interlining that is handled while still warm can be drawn out of shape, and the distortion only appears after the garment has been washed. Lay fused panels flat and let them reach room temperature before they travel to the sewing line. Dimensional behaviour after bonding is where the woven interlining's plain weave helps. With no directional stretch built into the construction, the fused panel does not grow or shrink against the shell, and the front edge stays even along its whole length. Watch for two things on the sample: a faint shine on the face where the press ran too hot, and a puckered seam allowance where too little pressure was used. Both are signs to adjust the process, not the article. 1. Cut a sample of the actual shell and a piece of interlining with the grain running the way it will run in the panel. 2. Fuse at the settings your line already uses for a comparable PA coated interlining, and write down the temperature, pressure and dwell time you ran. 3. Lay the bonded sample flat and let it cool completely before you judge hand, drape or bond strength. 4. Fold the sample over a table edge the way the finished panel will hang, and look for shine, strike-through or a hard ridge along the fold. 5. Run the sample through the laundering or dry-cleaning cycle the finished garment will meet, then check the face for bubbling and the edges for lifting. 6. Keep the approved swatch and its written settings with the style file, so the next reorder can be checked against a known reference instead of starting from scratch.
Workwear is a harder test than fashion. A uniform jacket is worn five days a week, laundered on an industrial cycle rather than at home, and expected to come back to the same shape for the life of the contract. The interlining inside it has to survive more cycles than the same article would ever see in a consumer fashion jacket. A bonded construction carries that load well. Because the interlining is fused across the whole panel rather than attached at points, there is no stitching line pulling the shape out of alignment and no pocket of air between the layers to bubble in the wash. The panel returns to its line after laundering instead of gradually going soft. Uniform programmes are also specified once and cut many times, in several sizes, across several production runs, often over a year or more. That puts a premium on an article that does not drift. Workwear shells tend to be firmer and heavier than fashion cloth, and the bond has to develop on that surface. Run the first panels on the actual uniform fabric and look at the edges and the collar stand after a full laundering cycle; those points show up a weak bond before anything else does. If the shell is very heavy, the support the garment needs may sit higher up our range than this article, and it is worth settling that before the specification is frozen.
| Article | 2054 |
| Composition | 100%Poly |
| Fabric format | Woven |
| Construction | 1/1 Plain Weave |
| Total weight | 23 gsm |
| Base fabric weight | 18 |
| Coating material | 100% PA |
| Glue weight | 5 |
| Bonding method | Fusible, activated on a standard fusing press |
| Colour | Off white / black |
| Roll width | 60" / 150 cm |
| Typical use | Lamination base for jacket fronts, collar stands, cuffs and pocket flaps |
Off white and black run as standard. Stock available; shipped by the container.
Before a bulk release, confirm the article, the shade and the roll width against the shell you will actually run, because the same construction reads very differently behind a pale poplin and a black twill. If a style needs a different grammage or a narrower roll, custom water jet interlining enquiries go to our technical team, who check what can be made in this construction before anything is quoted.
Roll length, packing and pallet arrangement are agreed per shipment — tell your sales contact how the rolls will be unloaded and stored at your end so the packing suits your handling. Current lead time, payment terms and shipping schedule are quoted with each order and should be confirmed when the booking is made, particularly where a container is being consolidated with other goods. For programmes running across a season, book the whole requirement against one article and one shade so the shipments match each other.
Bond failures are often blamed on the article when the roll is what changed. The adhesive on this water jet interlining is 5 gsm of PA over an 18 gsm woven base, and PA is hygroscopic: in a damp or humid store the coating draws moisture out of the air, and a roll that has done so no longer wets out the shell the way it did when it left the wrapping. The result reads like a material fault — a short bond, bubbles along the panel after the first wash, a faint shine where the press had to be run hotter to make the coating flow. In the store. Leave rolls in their original polythene wrap until the day they go on the cutting table, and stand them upright on a rack or cradle rather than laying them flat, because a roll stored flat under its own weight presses coating against cloth and can leave hard patches along the outer laps. A dry, shaded area off a concrete floor is enough — a pallet will do — and keep the stock away from exterior walls, roof leaks, steam lines, dyeing and finishing rooms, and anything giving off solvent. Sunlight and heat are the other enemy: a roll that has sat against a south-facing window or next to a boiler fuses unevenly along the laps nearest the source. Rotate first in, first out, and write the receipt date on each roll so the oldest goes to the press first. On the way to the line. A roll brought straight from a cold container or an unheated warehouse into a warm, humid cutting room will condense moisture onto the coating. Give it a day in its wrap to reach room temperature before you break the seal. Part-used rolls should be wrapped again rather than left open on the table overnight. If a fusible interlining has been in stock through a long, humid season, fuse a swatch from the outer laps and check the bond and the face before the roll joins a bulk run — a two-minute check that saves a panel.
We are a manufacturer rather than a trading company: production, quality control and stock sit under one roof, and we supply buyers worldwide — mostly converters, garment producers and trade partners who resell or specify our PA coated interlining into their own programmes. Fast-moving articles are kept in stock, so container-level repeat orders can be released without waiting on a fresh production run. Custom grammage, width and private-label packing are available on request, and we will help you match the right article to your shell fabric before you commit to bulk.